Effect of milling time on microstructure of Ti35Nb2.5Sn/10HA
biocomposite fabricated by powder metallurgy and sintering
تاثیر زمان آسیاب کردن بر ریزساختار بیوکامپوزیت Ti35Nb2.5Sn/10HA
تولیدشده با متالورژی پودر و زینترسازی
ABSTRACT
A new β-Ti based Ti35Nb2.5Sn/10 hydroxyapitite (HA) biocompatible composite was fabricated by mechanical milling and pulsed current activated sintering(PCAS). The microstructures of Ti35Nb2.5Sn/10HA powder particles and composites sintered from the milled powders were studied. Results indicated that α-Ti phase began to transform into β-Ti phase after the powders were mechanically milled for 8 h. After mechanical milling for 12 h, α-Ti completely transformed into β-Ti phase, and the ultra fine Ti35Nb2.5Sn/10HA composite powders were obtained. And ultra fine grain sized Ti35Nb2.5Sn/10HA sintered composites were obtained by PCAS. The hardness and relative density of the sintered composites both increased with increasing the ball milling time.